Wallace Instruments https://wallaceinstruments.com Fri, 25 Sep 2026 10:25:47 +0000 en-GB hourly 1 Press Release – Wallace Instruments Establishes First African Operation in Côte d’Ivoire https://wallaceinstruments.com/press-release-wallace-instruments-establishes-first-african-operation-in-cote-divoire Fri, 25 Sep 2026 10:09:05 +0000 https://wallaceinstruments.com/?p=2273 Press Release – Wallace Instruments Establishes First African Operation in Côte d’Ivoire

Wallace Instruments West Africa brings trusted, traceable quality measurement closer to natural rubber production

Dorking, UK, September 2026 – Wallace Instruments, the UK manufacturer of materials testing equipment, has established Wallace Instruments West Africa, a new company based in Abidjan, Côte d’Ivoire, marking a significant expansion of its support for the natural rubber industry in the region.

Wallace has a long-established customer base across West Africa, with natural rubber producers and processors relying on its instruments for plasticity, PRI and viscosity testing. The new operation brings Wallace servicing, calibration, spare parts and technical expertise closer to those customers, reducing turnaround times and establishing a local presence from which to build long-term relationships.

Côte d’Ivoire is West Africa’s leading natural rubber producer and has become one of the world’s largest exporters of technically specified rubber (TSR), serving tire and rubber product manufacturers around the globe, including the Americas. Well-maintained, calibrated instruments produce consistent, traceable results at source that benefit the entire supply chain by providing greater confidence in the quality behind every shipment.

The new facility will include a laboratory and training center, giving existing and prospective customers a place to see Wallace equipment in operation and access hands-on testing and technical guidance. Wallace Instruments West Africa technicians are trained by Wallace and equipped with the OEM calibration kits required for complete and compliant calibration, while customs-cleared stocks of spare parts held in Abidjan will reduce lead times.

The company will also work with an exclusive local partner to offer servicing and calibration for other equipment used across plantations and processing facilities in West Africa.

“Our aim is to bring trusted, traceable quality measurement closer to natural rubber production,” said Wallace Instruments Managing Director Chris Norval. “Establishing Wallace Instruments West Africa helps our customers maintain reliable testing and strengthen quality control, while giving the wider supply chain greater assurance in the test data. We’re excited to be building our team locally and look forward to growing with the region.”

************************************************************************************

ABOUT WALLACE INSTRUMENTS

For more than 75 years, Wallace Instruments has designed and manufactured precision testing equipment for the rubber and plastics industry. Its product range covers plasticity, viscosity, hardness, density, compression and flex testing, as well as laboratory aging and specimen preparation equipment, supporting research and quality assurance in natural and synthetic rubber production as well as tire and rubber product manufacturing.

Its equipment is designed and manufactured in the United Kingdom by Tenon Engineering, a sister company that also supplies other world-leading scientific instrument manufacturers.

Both companies are based in Dorking, Surrey.

Contact information: George Bates ([email protected])

For more information on this press release contact:

David Cawthra | Gail Reader

RUBBER HEART Ltd
The Townhouse, 114 – 116 Fore St, Hertford, SG14 1AJ, United Kingdom
T: +44 (0)7825 232601
T: +44 (0)7968 081261
E: [email protected]

www.therubberheart.com

]]>
Paper 3 – Importance of Experimental Parameters on Rapid Plasticity Testing for PRI (Plasticity Retention Index) https://wallaceinstruments.com/paper-3-importance-of-experimental-parameters-on-rapid-plasticity-testing-for-pri-plasticity-retention-index Mon, 06 Jul 2026 14:29:20 +0000 https://wallaceinstruments.com/?p=1888 Continue reading "Paper 3 – Importance of Experimental Parameters on Rapid Plasticity Testing for PRI (Plasticity Retention Index)"]]> Paper 3 – Importance of Experimental Parameters on Rapid Plasticity Testing for PRI (Plasticity Retention Index)

R. Morgans1, S. Lackovic2, B. McGarry2, G. Dinnage2, B. Pearce2

  1. University of Greenwich, School of Engineering, Medway Campus, Pembroke, Chatham Maritime, Kent, England, ME4 4TB, UK
  2. H. W. Wallace & Co. Ltd, Curtis Road Industrial Estate, Curtis Road, Dorking RH4 1EJ, UK

Abstract

Rapid plasticity is one of the basic tests used in the natural rubber industry and is the measurement of compression of a specimen of known thickness at a known temperature under a predetermined load for a known time. The Plasticity Retention Index is a measure which reflects the resistance of natural rubber to thermal oxidation. Several parameters affect the end result, such as platen parallelism, platen temperature, force, time, the centralisation of the sample, the type of paper/material used between the platens and sample and the ageing temperature and time.

This paper aims to demonstrate the effect of these parameters on the final end result.

Experimental work was carried out using the current Rapid Plastimeter (P12E) and the new Wallace Cogenix Rapid Plastimeter (P14). The new P14 enabled the platen temperature and test times to be accurately varied and controlled. The effects of sample positioning and the type and thickness of paper used between the platens and sample was also investigated.

The P14 instrument enables tighter temperature control, allowing the effects of temperature to be investigated.

Introduction

Use of the equipment and parameters specified in the current standard define Rapid Plasticity (ISO 2930:1995 – ref. 1). In general, a plastic material is one which, when subjected to a force, continues to deform as long as the force acts with much (or all) of the deformation remaining when the force is removed (ref. 2). Rapid Plasticity is defined by measuring the compression of a specimen of specified thickness at a specified temperature under predetermined loading for a specified time. Samples are sandwiched between a carrier paper to protect the platens from contamination. One Wallace Rapid Plasticity unit represents a change in thickness of 0.01mm (ref. 3). The current standard specifies a method for the rapid determination of the plasticity of raw rubber and non-vulcanised rubber compound.

Rapid Plasticity has remained one of the basic tests in the Rubber Industry for the past 50 years. The original Wallace Rapid Plastimeter (P1 – developed in 1951) used steam-heated platens and relied on a dial gauge, a stopwatch and the skill of the operator to produce results. The arrival of the microprocessor lead to the P12 instrument – first introduced in 1984. The P12 retained the steam driven platens but used a sensor to measure distance and the microprocessor to time the test; the load was spring-driven. The current production instrument (P12E) was introduced in the late 1980’s and uses electrically heated platens1 and an accurate load application method; the P12E still relies on operator skill to calibrate the platen gap. The new P14 Rapid Plastimeter builds on the previous instruments and includes several new features. These include the use of platinum resistance sensors to measure the temperature of both platens; operator error is reduced by a semi-automatic gap-calibration procedure.

The Plasticity Retention Index of a sample is the ratio of the rapid plasticity numbers after ageing at 140°C and before ageing, multiplied by 100. The PRI test requires the use of a plastimeter and ageing oven. The current production oven (O12) was introduced to accurately heat the samples to 140°C. However, the temperature is not indicated but is fixed by adjusting the temperature set point. The new O14 (to complement the new P14) makes use of a platinum resistance thermometer together with a 3 term temperature controller to accurately control the temperature to 140° ± 0.2°C. The standard (ref. 1) requires an ageing time of 30 mins ± 0.25 mins. The standard (ref. 1) specifies limits and acceptable ranges for each of the parameters affecting the end result; some of these originate from the era of the P1. This paper investigates some of these parameters and limits with the advent of more accurate instrumentation. A practical appreciation of their effects may be used to produce accurate, consistent results. This paper incorporates previously unpublished work from H W Wallace and surveys other literature on the subject.

Method

All data were taken with a resolution of 0.1 plasticity units and recorded with a resolution of 0.5 units. A median result was taken from 3 measurements.

Platen Temperature Variation

Platen temperature dependence was studied by adjusting the temperature of both top and bottom platens either side of the standard temperature (100°C). The temperature was measured using the temperature probe mounting supplied in the instruments’ calibration kit, which is traceable to national standards.

Sample Centralisation and Platen Parallelism

Sample centralisation was investigated by placing samples at various off-centre positions on the platen face. The affect of platen parallelism was studied, by adjusting the tilt (Figure. 1) of the top platen from 0° to 0.65° and 1.3° respectively.

Figure 1 Diagram (exaggerated) showing top platen at an angle to the bottom  platen
Figure 1 Diagram (exaggerated) showing top platen at an angle to the bottom platen

Operator Dependence and Instrument to Instrument Variation

Operator result dependency was tested by using 5 members of staff. Their instrument knowledge ranged from an operator with several years of inspection experience through to one with no previous experience.

Instrument to instrument variation was examined by analysing the historical inspection/calibration reports produced on P12E instruments that used common rubber batch samples.

Sample Paper Dependence

Testing was carried out by using different types of material and paper between the platens and sample. Materials tested include standard paper, photocopier paper, tracing paper, toilet tissue, aluminium foil and brown paper. In addition to varying the type of material, each was tested at the standard size (35mm square) and at 16 and 14.5mm square.

Load Variation

The load applied to the sample was investigated by adjusting the force either side of the standard force (100N).

Results

The natural rubber used to perform the tests normally has a graduation in plasticity value across the sheet. Since the same sample cannot be tested more than once, the results had to be made using different, but adjacent, samples of the test rubber. Some variation in the results can be attributed to these variations in the sample. Previous experience with a number of instruments suggests that the variation with similar material is normally about ±1.5 plasticity units across the sheet.

Platen Temperature Variation

The temperature specified by the standard is 100 ±1 °C. At 101°C and 99°C, the results were comparable to the standard results at 100°C. Individual results did however, appear to exhibit slightly more fluctuations than usual about the median. At 102°C (1°C above the top limit) the results were approximately 1 plasticity unit lower. At 98°C (1°C below the bottom limit) there was a 1 unit increase in plasticity. At 95°C there were more fluctuations in the results and approximately a 1.5 unit increase in the plasticity number (Table 1).

Previous work (D. A. Hills, ref. 4) enforces these findings; the results showed that the plasticity number will be increased by approximately 2 units for a drop in temperature of 6°C from the standard 100°C platen temperature. Reliable results will only be obtained if the platen temperatures are kept within close limits.

Temperature (°C)Median Results (plasticity number)
10231.030.531.0
10130.531.531.5
10031.031.032.0
9931.531.031.5
9832.032.032.0
9532.032.533.0

Sample Centralisation and Platen Parallelism

Centralisation of the sample is important. Generally, it is unlikely that the operator will place the sample exactly in the centre every time. A few millimetres deviation from this point does not measurably influence the results. However, once the top platen compresses the edge of the sample (corresponding to about 5 mm off-centre) the plasticity number drops by approximately 1 unit – the result of using the same compression over a reduced sample surface area. Results will continue to drop as less of the sample is used.

With 0.65° tilt on the top platen (from the standard parallel position – see Figure. 1), results are consistently reduced by 1 plasticity unit. Tilting the platen to 1.3° tilt reduces the result by 2 units (see Table 2). The results will eventually drop to zero as the tilt is increased.

Angle of tilt (°)Median Results (plasticity number)
0.0033.032.533.032.5
0.6532.032.032.031.5
1.3031.031.031.531.0

Operator Dependence and Instrument to Instrument Variation

Note that it was necessary to train the inexperienced operators (for about 5 minutes) before testing. It is virtually impossible for an untrained operator to produce a reliable result. The results were then consistent between operators (see Table 3), with a variation of ±0.5 plasticity units.

The instrument to instrument variation was examined by analysing the last 10 inspection/calibration reports produced on P12E instruments. The same batch of rubber was used in all cases. The variation was found to be minimal and can be seen in the distribution curve (Figure 2).

OperatorResults (plasticity number)
133.033.033.0
233.032.533.0
333.032.532.0
432.032.533.0
533.033.533.0
Figure 2. Graph showing instrument to instrument variation
Figure 2. Graph showing instrument to instrument variation

Sample Paper Dependence

Tissue paper or cigarette paper of about 22g/m2 cut into two equal pieces should be used (refer to ISO standard, ref. 1). However, it is known that the recommended method is not always used. Measurements have been made using different sizes and types of material between the rubber sample and platen.

The instrumental results are very dependent on this parameter. When the size of the material is halved (using the recommended standard cigarette paper), the paper does not rest on the shield around the bottom platen. This reduces the test results by about 4 units. Thus, for this reason, the position of the paper becomes more important if larger sample papers are used.

The other materials used (10 in total) made a difference to the final result (see Table 4). The differences ranged from a few units below to more than 10 units above the standard result. It can be seen that although the numerical value of the result varies between different material types for the first group of materials, the results are reasonably consistent for any one material.

Material no.Results (plasticity number)
Cigarette paper36.537.036.0
Hand towel paper33.035.034.0
Hard toilet tissue35.037.036.5
Wrapping film38.038.036.0
Toilet tissue46.544.045.0
Photocopier paper53.043.049.0
Tissue paper52.053.051.5
Tracing paper49.057.052.0
Brown paper59.558.057.0
Mylar film32.533.034.0
Cling film23.022.023.0

Load Variation

The load specified in the standard is 100 ±1 N. At 101 N and 99 N, there was no significant variation from the standard results (when applying a force of 100 N). At 102 N (1 N above the top limit) the results were about the same as at the top limit. At 103 N (2 N above the top limit) the results were approximately 1.5 units below the standard result. At 98 N (1 N below the bottom limit) the results were approximately the same as at the bottom limit. A force of 97 N (2 N below the bottom limit) gives results approximately 1.5 units above the standard result. These results are tabulated in Table 5. This demonstrates that it is important to check the load calibration.

Force (N)Median Results of a typical sample (plasticity number)
10330.5
10231.0
10131.0
10032.0
9932.0
9832.0
9733.5

Conclusion

It has been demonstrated that several parameters can affect the plasticity value obtained from a given sample. Results are very repeatable, provided these parameters are controlled. In practice, it has often been found that results are simultaneously affected by the variation of more than one parameter.

Tight temperature control is important. The platens of the obsolete P1 and older P12 instruments were steam heated – leading to large temperature variations in some cases. The P12E platens are electrically heated, and must be checked and adjusted regularly (which is often not the case). The measurement method and lack of care in setting the P12E’s platen temperatures can lead to significant variations from the 100±1 °C specified in the standard. The new P14 deals with these problems by using an accurate sensor to measure the platen temperature, and by incorporating a calibration point near to the platen surfaces. Care must be taken to ensure that the same temperatures are used for both platens, since this will effect the end results.

Centralisation of the sample is important, but normal care is adequate. Lack of platen parallelism also affects the result. This is particularly so when the alternative platen sizes allowed in the standard are used – i.e. the parallelism must be reset every time the platen has been changed. In addition, care must be taken to ensure that the correct platen sizes are used as this will effect the results obtained.

Once trained, operator dependence is not important. The instrument to instrument variation is low and within the spread of a ‘uniform’ sample sheet.

The dependence of the result on the sample paper used is important. Use of the paper recommended by the standard will ensure that results are consistent. Other sample carriers may be used (after validation) and will produce different, but consistent results. The paper size is also important and if larger sample papers are used, the effect of the heat-shield can lead to significantly low readings.

Sample size is important. The standard must be adhered to; other sizes must not be used. The sample preparation equipment supplied with the instrument ensures this.

The load is accurately applied only in the P12E and P14 instruments – with a calibrated weight arm applying the load. It is worth noting that the geographical variation in gravity can lead to differences of up to 0.5%. This accounts for almost half of the allowable tolerance in the standard. Therefore it is recommended that the weight arm is calibrated locally at any particular location in the world.

Use of the P1, timed by the operator, can lead to highly significant variations in the final result. Figure 3 demonstrates that a variation of ±1 second in the time of application of the test force can make a difference to the final result by as much as one plasticity unit. The crystal controlled timing of the P12, P12E and P14 ensure that the result timing is accurate and exact. Regular servicing of the instrument will ensure that all parameters are set accurately within the limits specified in the standard to maintain accurate and reliable results.

PRI Measurement

The PRI test requires the use of a plastimeter and ageing oven and so in addition to the results being affected by the parameters discussed above, the PRI result may also be affected by the oven. As in the case of the requirements for tight temperature control of the plastimeter platens, the ageing oven also requires tight temperature control. Previous work (E.D. Farlie and H. W. Greensmith – ref. 5) indicates that a temperature variation of ±1°C from the standard 140°C can produce a difference in the PRI value of ±3 units for a PRI of approximately 50. As a result, the standard (ref. 1) specifies the tolerance to be ±0.2°C to maintain the accuracy. The standard also states that a variation of ±0.5°C may be used but this may impair the accuracy of the results. The new oven, O14, uses an accurate platinum resistance thermometer to measure and control the temperature.

Additionally, previous work (ref. 5) also suggests that rubber plasticity falls continuously but at a decreasing rate with increasing ageing time. Consequently, a variation in the ageing time of a few minutes is likely to effect the result by a few units (the exact deviation is dependent on the type of rubber sample). The standard (ref. 1) specifies the ageing time within close limits (± 0.25 mins) to ensure reliability and repeatability.

References

  1. ISO 2930, Determination of the plasticity retention index (PRI) of raw natural rubber, 1995.
  2. RABRM Bulletin, Special Issue on Plasticity (1954). Vol. 8, No. 4.
  3. McGarry, B. M., Rapid Plasticity and Plasticity Retention Index Testing (1994).
  4. Hills. D. A. (1964), Rubber Journal, Testing with the Wallace Rapid Plastimeter.
  5. Farlie. E. D. & Greensmith. H. W., Transactions of I.R.I, 1966, 42, Part III.

Download Paper

]]>
Press Release – Wallace Instruments Releases Major Software Upgrade for Hardness and Plasticity Testing https://wallaceinstruments.com/wallace-instruments-releases-major-software-upgrade-for-hardness-and-plasticity-testing Mon, 29 Jun 2026 17:08:48 +0000 https://wallaceinstruments.com/?p=1976 Press Release – Wallace Instruments Releases Major Software Upgrade for Hardness and Plasticity Testing

For Rubber World GPS Show Daily – September 2025

Dorking, UK – Wallace Instruments, a leading manufacturer of rubber testing equipment, has released a major software upgrade covering its range of Shore and IRHD hardness testers, as well as the Rapid Plastimeter Mk V (P14). Developed to support data traceability, simplify workflows and improve day-to-day lab operations, the new platform offers a more intuitive and connected user experience across key Wallace instruments.

The upgrade introduces an improved interface that enables multiple Wallace instruments to connect to a single server, allowing multiple operators to work simultaneously. Each user has a secure login and access to customized workflows, including traceability fields such as batch ID, material type or polymer reference. All test results are securely stored on the server, and users can review and filter results on screen, then export single or multiple files in CSV or PDF format for integration with laboratory records and quality systems.

The software offers significant improvements in ease of use and lab productivity. It includes standard test templates while supporting custom configurations, giving labs the flexibility to adapt testing protocols to their own procedures. The system is designed to be efficient, practical and future-ready making it easier to train users, manage data and scale across testing teams.

“Hardness and plasticity testing are essential to elastomer quality assurance,” said Chris Norval, Managing Director of Wallace Instruments. “This upgrade delivers what today’s labs are asking for – a system that’s secure, adaptable and straightforward to use. It supports routine testing while making it easier to manage data, improve workflows and keep productivity high.”

Visitors to the Global Polymer Summit can see the new system in action at Booth 1010.

************************************************************************************

ABOUT WALLACE INSTRUMENTS

With more than 75 years of experience, Wallace Instruments supplies industry-leading materials testing equipment specializing in measuring physical properties such as hardness, plasticity, viscosity, cure, and compression. Millions of tests are conducted annually on Wallace instruments worldwide, supporting research and quality assurance in sectors such as natural and synthetic rubber production, as well as tire and rubber product manufacturing.

Its equipment is designed and manufactured in the UK by Tenon Engineering, a sister company that also supplies other world-leading scientific instrument manufacturers. Both companies are based in Dorking, Surrey, United Kingdom.

Contact information: George Bates ([email protected])

For more information on this press release contact:

David Cawthra | Gail Reader

RUBBER HEART Ltd
The Townhouse, 114 – 116 Fore St, Hertford, SG14 1AJ, United Kingdom
T: +44 (0)7825 232601
T: +44 (0)7968 081261
E: [email protected]

www.therubberheart.com

]]>
Shows We’re Exhibiting At… https://wallaceinstruments.com/shows-were-exhibiting-at Thu, 25 Jun 2026 15:10:04 +0000 https://wallaceinstruments.com/?p=1928 Please see the exhibitions we’ll be attending this year:

15th – 17th September – Shanghai

Booth N2A111

Our head engineer Gordon Hold will be joining our regional Sales & Service agent George Sun, of Sharonus (Beijing) Tech Co. Ltd., to share our latest updates with customers. With our range of hardness testers and software available to demonstrate on the stand, make sure you stop by and see how Wallace Instruments can help you manage the cost of quality.


29th – 30th September – Louisville

Booth 525

For the fourth year in a row Wallace Instruments will be exhibiting at the Global Polymer Summit. It’s a great opportunity for us to speak with our customers in North America and highlight the after sales support available from our Ohio based agent, Leverett Anderson. We can’t wait to get to Louisville and discuss your requirements with you.


Past Shows

7th – 10th April – New Delhi

Booth I013

Once again our regional sales and service partner Alfatek Services will be exhibiting Wallace Instruments range of testing solutions to customers in India. This show is a constant fixture on our calendar and a great opportunity to understand the local market.


10th – 12th June – Ho Chi Minh City

Booth R36B

Alongside our local agent Nhat Minh Equipment & Chemicals Co., Wallace Instruments will be attending Rubber & Tyre Vietnam in June. With a long tradition of supplying rubber testing equipment to South East Asia, this is a great opportunity to see our range of instruments. From natural to black rubber we have equipment to make your testing as accurate and simple as possible.


]]>
Press Release – Wallace Instruments launches WAS3 Pneumatic Cutting Press for safer, more consistent specimen preparation https://wallaceinstruments.com/press-release-wallace-instruments-launches-was3-pneumatic-cutting-press-for-safer-more-consistent-specimen-preparation Wed, 24 Jun 2026 16:27:10 +0000 https://wallaceinstruments.com/?p=1854 May 2026

Wallace Instruments launches WAS3 Pneumatic Cutting Press for safer, more consistent specimen preparation

Featured In

Rubber World Tyre Trends

Wallace Instruments launches WAS3 Pneumatic Cutting Press for safer, more consistent specimen preparation

Dorking, Surrey, UK – Wallace Instruments, a globally recognised leader in rubber testing equipment, has launched the WAS3 Pneumatic Cutting Press, expanding its UK-manufactured specimen preparation range.

Pneumatic cutting presses offer significant advantages over manual alternatives in laboratory and production environments. Consistent cutting force is applied with every cycle, regardless of operator strength or fatigue, reducing variability in specimen quality across a working day or between different technicians. This consistency matters: poorly cut specimens – with ragged edges, inconsistent dimensions, or stress introduced during cutting – can compromise test results. Pneumatic operation also reduces the repetitive physical effort associated with manual pressing, supporting operator wellbeing over long production runs.

The WAS3 has been developed to deliver these benefits with a particular focus on practical safety. It is designed for single operator use with a two-button activation system that requires both buttons to be pressed within half a second, ensuring the press cannot be activated while the operator’s hands are in the cutting area. Protective guards on three sides further support safe operation.

Providing 15kN of cutting force, the WAS3 can cut through 10mm thick 95 Shore A rubber sheet with ease. It operates using a pressure of 5.0 bar from a filtered air supply and delivers consistent, user independent cuts without physical exertion, making it suitable for all technicians. The WAS3 is compatible with existing Wallace cutting dies, allowing laboratories to integrate it into their workflows without replacing their existing die sets. Its compact footprint fits easily into both laboratory and production environments.

“Specimen preparation is the foundation of accurate rubber testing,” said Chris Norval, Managing Director of Wallace Instruments. “With the WAS3 we focused on practical safety, dependable cutting performance and drop-in compatibility. Labs get a compact pneumatic press that fits the air lines already in place, uses their current Wallace dies and delivers consistent results for every operator – because when specimen quality is controlled, you can have confidence in the results that follow.”

For more information about Wallace Instruments and its range of products, visit www.wallaceinstruments.com

ABOUT WALLACE INSTRUMENTS

With more than seventy-five years of experience, Wallace Instruments supplies industry leading materials testing equipment for measuring hardness, plasticity, viscosity, cure and compression. Millions of tests are performed annually on Wallace instruments worldwide, supporting research and quality assurance in natural and synthetic rubber production as well as tire and rubber product manufacturing.

Its equipment is designed and manufactured in the United Kingdom by Tenon Engineering, a sister company that also supplies other world-leading scientific instrument manufacturers. Both companies are based in Dorking, Surrey.

Contact information: George Bates ([email protected])

For more information on this press release contact:

David Cawthra | Gail Reader

RUBBER HEART Ltd
The Townhouse, 114 – 116 Fore St, Hertford, SG14 1AJ, United Kingdom
T: +44 (0)7825 232601
T: +44 (0)7968 081261
E: [email protected]

www.therubberheart.com

]]>
Paper 1 – Comparison of results and test methods using the Micro IRHD and the Micro Shore rubber hardness measurement instruments https://wallaceinstruments.com/comparison-of-results-and-test-methods-using-the-micro-irhd-and-the-micro-shore-rubber-hardness-measurement-instruments Wed, 24 Jun 2026 13:46:34 +0000 https://wallaceinstruments.com/?p=1815 Comparison of results and test methods using the Micro IRHD and the Micro Shore rubber hardness measurement instruments

R. Morgans1 BSc, S. Lackovic2 BSc, PhD, P. Cobbold2

  1. School of Engineering, University of Greenwich, Medway Campus, Chatham Maritime, Kent, ME4 4TB, UK
  2. H W Wallace & Co. Ltd, Curtis Road Industrial Estate, Curtis Road, Dorking RH4 1EJ, UK

Abstract

Rubber hardness can be determined using either the IRHD (International Rubber Hardness Degree) or the Shore Scale. The test methods and instrumentation for each are distinctly different, for example in the time and method of indenter application and geometry. This paper is concerned with the micro versions of these test methods – normally used to measure small samples. Instrumental parameters and sample limitations of both methods were investigated. The paper illustrates the practical differences between the tests, their limitations and the effects on the results obtained, providing valuable information of the advantages and disadvantages shown by each test method.

Introduction

Hardness measurement is one of the most commonly used methods in product testing and quality control. Two test scales are commonly used, providing results on either the IRHD or Shore scale. A number of instrument types exist for both – the IRHD dead load and Shore-A scales are most commonly used for rubber. Both methods are described in international standards.

The IRHD test is usually non-destructive, and as such has to be the preferred method for final product inspection; the test takes 35 seconds. In contrast, the Shore method is often destructive (leaving a permanent indentation), but only takes 1 (or 3) seconds. It is recognised that although there is little relationship between the two tests, there can be a degree of correlation over certain hardness ranges for some compounds. Both methods have been used for decades, yet Briscoe and Sebastian1 (1993) report that the Shore-A test has not been subjected to the sort of detailed analysis of the IRHD method. Their paper looks at the Shore-A test and concludes with an approximate relationship of Shore-A and dead load IRHD hardness. Brown and Soekarnein2 carried out work in 1991 investigating the reproducibility of Rubber Hardness Tests on both the IRHD and Shore-A scales. The instruments used were analogue, lacking the precision of modern electronic models.

The IRHD scale has a micro counterpart – for which a standard has existed for over 30 years (ISO 483 & ASTM 14154). The proposed Shore Micro does not yet have a released standard. The Micro IRHD instrument was devised in the 1950’s as a scaled down version of the dead load for testing thinner, smaller samples and products (such as ‘O’ rings). The Micro IRHD results are generally comparable to those given by the standard dead load IRHD instrument. In contrast, there are various ‘Shore-M’ scale hardness testers appearing on the market. The results are not comparable to those given by the Shore-A scale. Also, little is known about the Shore-M scale, its relationship to the Micro IRHD scale and instrumental differences.

This paper is concerned with both micro instruments. Experience has shown that, in practice, a degree of confusion exists between users of the two test methods. Also, it is not always possible for tests to conform exactly to a standard due to sample size and shape constraints. Whilst comparing the two methods, the paper’s objective is not to determine a relationship between the micro scales, but to illustrate the practical differences between the tests, the results obtained and some of the instrumental parameters involved.

In order for this paper to be written, Wallace manufactured a Shore-M instrument, to currently available information. This instrument is compared to the standard Wallace Micro IRHD hardness tester.

Differences between the Micro IRHD and Shore-M Instruments

The Micro IRHD instrument uses a spherically tipped indenter. A sharp conical indenter is used for the Shore-M instrument.

The micro IRHD is based on the use of dead loads. The test uses a foot to hold the sample in place with a force of 245mN. A primary load of 8.3mN is then applied for 5 seconds, providing a datum position. A secondary load of 145mN is then applied for 30 seconds. The incremental displacement (from the datum) is measured and converted to an IRHD value (a non-linear scale defined in the standard). The maximum indentation depth is 0.3mm.

In contrast, the Shore-M test uses a calibrated spring (applying varying forces of between 0.3N and 0.8N) to supply an indentation force and the indentation force increases linearly with indenter displacement. The presser foot applies a force sufficient to overcome the spring force. Once the presser foot contacts the sample, the indentation depth is recorded after a set time. The maximum indentation depth is

1.25mm. The standard dwell times for the Shore-A scale are 1 and 3 seconds. These are also used for the Shore-M test. Each durometer point on the Shore-M scale represents 0.0125mm displacement.

Experimental

The Wallace Micro IRHD and Shore-M instruments were calibrated before starting the test sequence and rechecked at the end. The standard temperature of 23 ± 2°C was used, except where otherwise noted. Each test was carried out on the Micro IRHD and the Shore-M instruments in sequence, with the Shore-M instrument using either a 1 or 3 seconds dwell time (timed to ± 0.1 s). Each sample was tested in 5 different places.

Four standard Wallace test blocks* covering the range 40 to 80 IRHD were used to provide comparative results for each instrument. Additionally, a variety of rubber samples were tested on both instruments. The nature of the micro test implies the use of small samples. The effects of sample thickness were investigated by carrying out tests on thinner samples. Although ISO 483 allows 1mm thick samples to be used, the preferred thickness is 2 ± 0.5mm and the standard recommends that two or more samples be plied together to conform to the requirements. It is known that the Shore-M scale has similar requirements. Tests were performed on 1, 2 and 3mm thick samples. A latex surgical glove of 0.1mm thick was used as a sample with up to 15 pieces plied together in incremental steps to determine the effect on the results.

The Wallace test blocks are approximately 25mm ´ 25mm. To meet the standard3, the indenter must be at least 2mm from the edge of a test piece. This requirement was investigated by reducing the size of a standard sample (initially quartered and then reduced by regular amounts). Since 5 tests are performed on each sample, the minimum size sample required to conform to the standard is approximately 6 ´ 6 mm. The sample was further reduced to measure the effects of decreasing the size below the standard specifications.

A bent sample can give an apparently softer result since the load deflects the sample before indentation occurs. The foot force of the Shore-M scale is much larger and this effect was examined on both instruments.

The effects of temperature on the test was compared by operating both instruments at 33 ± 2°C. Both instruments and samples were kept in the same environment.

Since tests may be conducted on a previously measured spot, the effect of repeated measurements on the same spot was investigated for both instruments.

Since it is known that in the case of the Shore-M instrument the foot load simply needs to overcome the spring force, it was decided to investigate the effect of altering the applied foot force (presser foot weight). The Shore-M foot force was applied by a 514g weight; this was reduced to 152.5g. Weights were added in increments of 50g to a maximum of 350g, applying a total weight of 502.5g. Tests were carried out on the standard Wallace blocks at each increment. A microscope was used to view the indentations (immediately after testing and after elapsed time) produced on different samples using both instruments.

* The standard Wallace test blocks are varying compounds of natural rubber, supplied by MRPRA.

Results

Standard Test Blocks

Figure 1. Increasing deviation between IRHD and Shore scales with increasing hardness

The standard Wallace blocks* gave repeatable results on both instruments. The 1 and 3 second Shore-M dwell times produced equivalent results with an increasing tendency to deviate from the IRHD result with increasing hardness values. See figure 1.

Variations between different sample trays

Table 1. Samples tested with their standard deviations
Table 1. Samples tested with their standard deviations

Generally, different rubber samples gave repeatable results (table 1) on both instruments. Additionally, the average results were consistent between instrument types and Shore dwell times. However, some anomalies were noticed when testing with the IRHD instrument. These were found to be due to imperfections in the sample and the samples’ lack of flatness. In contrast, the same effects were not seen with the Shore-M results.

H An example of an anomaly due to sample imperfections and the sample’s lack of flatness.

Effects of Thickness

Figure 2: Example of decreasing hardness with increasing thickness for an unspecified rubber type
Figure 2: Example of decreasing hardness with increasing thickness for an unspecified rubber type

As expected, different results were obtained with 1mm, 2mm and 3mm thick samples. There was a general decrease in hardness value with increasing thickness, but all results were repeatable. See figure 2.

Figure 3. Increasing the thickness of a latex surgical glove of initial thickness of 0.1mm
Figure 3. Increasing the thickness of a latex surgical glove of initial thickness of 0.1mm

When testing samples of 0.1mm thickness, more than one piece was plied. Generally, the results of each plied thickness deviated little from the mean although a few anomalies were noted. These are believed to be due to the number of tests carried out on the top piece of rubber and samples flatness. The sample hardness value decreased with increasing thickness. Initially, the Shore-M results were about 10 IRHD units higher than those produced on the Micro IRHD, but once the sample thickness increased to 1.54mm, the results were comparable (Figure. 3).

Effects of Lateral Sample Dimensions

Figure 4. Extreme differences in results between IRHD and Shore-M tests when reducing the dimensions of a sample of about 40 IRHD.
Figure 4. Extreme differences in results between IRHD and Shore-M tests when reducing the dimensions of a sample of about 40 IRHD.
Figure 5. Extreme differences in results between IRHD and Shore-M tests when reducing the dimensions of a sample of about 74 IRHD
Figure 5. Extreme differences in results between IRHD and Shore-M tests when reducing the dimensions of a sample of about 74 IRHD

Despite reducing the sample size, the results on both the instruments were found to be repeatable. The results on the Micro IRHD were generally consistent for the softer rubber (40 IRHD). However, the Shore-M instrument gave rapidly increasing hardness values with decreasing sample size (up to a maximum difference of approximately 15 units). Although the 50 IRHD sample gave similar results, the Micro IRHD tended to produce decreasing hardness values with decreasing dimensions (to a maximum hardness difference of 3.5 units). In contrast, the Shore-M results exhibited the same upward trend as before (but with a reduced maximum hardness difference of approximately 7 units). The 65 IRHD sample tested on the Micro IRHD decreased at the same rate as before, while the Shore-M instrument exhibited more stable results despite a few fluctuations. Finally, the hardest sample tested (70 IRHD) on the Micro IRHD instrument exhibited a general downward trend (a maximum difference of approximately 4 IRHD). Conversely, the Shore-M instrument produced more stable results between the dimensions tested, with a slight upward trend, of about 1.5 units. The two figures below (fig. 4 and fig. 5) show the extreme cases as discussed above, namely the softest and hardest rubbers

Effects of Sample Flatness

Figure 6. Harder samples being more affected by bending than softer samples
Figure 6. Harder samples being more affected by bending than softer samples

Tests were carried out on bent samples to determine the effects on both instruments. These tests showed that for softer rubbers (40 and 50 IRHD), the samples quickly recovered to the ‘flat’ state and there was little difference between IRHD and Shore readings. For harder samples (60 and 70 IRHD), the Shore-M instrument gave consistent results, independent of the state of the sample, but the Micro IRHD instrument gave much lower values. In an extreme case, a 70 IRHD sample showed a difference of 30 IRHD between its ‘flat’ value and ‘bent’ values. In fig 6 below, each collection of 3 points is for each of the 4 standard Wallace blocks. In each case, the first of the three points is a test on an unbent sample, the second is a test on a previously flexed sample and the third is a test on a sample which has been kept bent for 10 minutes.

Effects of Temperature

Increasing the temperature to 33 ± 2°C made little difference. The softest sample (40 IRHD) didn’t show significant changes on either instrument. The 60 and 70 IRHD samples exhibited a decrease in hardness of 1.5 units on the Micro IRHD and 0.8 units on the Shore-M. The hardest sample (80 IRHD) exhibited the greatest effect, showing a decrease of 2.4 units for the Micro IRHD instrument and a decrease of 1.5 units for the Shore-M instrument. Observations were made on a variety of samples and although repeatable results were obtained, no general trends were observed with increased temperature

Effects of Repeated Testing in One Location

Figure 7. Repeated testing in one location
Figure 7. Repeated testing in one location

The same spot was repeatedly measured. There was a decrease in hardness with increasing number of tests shown on both instruments. However, the Micro IRHD instrument gave more stable results, with only a total decrease of 1.5 IRHD over 28 tests on a rubber of approximately 65 IRHD. In contrast, the Shore-M instrument results decreased much more rapidly before levelling out. The total decrease was approximately 5 units over 28 tests on the same sample. It was also noted that results produced from 1 second dwell time were consistently lower than those produced with a 3 second dwell time on the same sample. These results are represented graphically in figure 7 below.

Effect of Altering the Shore-M Foot Force

In general, increasing the foot force appeared to produce increasing hardness. The effects were small on the samples tested.

Observations of the Sample Surface After Testing

Figure 8. Photograph of an indentation left on the fluoro compound after being tested on the Shore-M. The magnification used here is 350X.
Figure 8. Photograph of an indentation left on the fluoro compound after being tested on the Shore-M. The magnification used here is 350X.

Although all samples previously tested were observed for surface effects, particular attention was paid to a small selection, namely silicone, a fluoro compound, EPDM, a chloro compound and the standard Wallace test blocks. Immediately after testing, the indentation left by the Micro IRHD instrument can be seen by eye. After a few minutes the indentation disappears, illustrating the non-destructive nature of the Micro IRHD test. In contrast, the samples tested on a Shore-M instrument exhibited a clear indentation immediately after testing both to the eye and under the microscope (see fig. 8). These indentations were also observed about 2 hours later. The same indentations can still be seen a week later, demonstrating a permanent deformation experienced by samples tested on a Shore-M instrument.

Discussion

As expected, very thin samples of non standard thickness influenced the results taken on both instruments. This is due to the influence of the supporting table and with increasing sample thickness, the effect becomes less apparent.

While the Micro IRHD results remained essentially constant for all lateral dimensions and hardnesses values tested, the Shore-M results showed that the apparent hardness rapidly increases for decreasing sample dimensions on the softer rubber, but less so for harder samples. Again the Micro IRHD exhibits a clear advantage.

The degree of sample ‘bend’ is important and its’ different effects are very much apparent between the two instruments. Harder rubbers are more affected by lack of flatness on a Micro IRHD instrument, due the small foot force involved. None of the Shore-M results exhibit fluctuations, since the foot force is large enough to flatten the sample, displaying a clear advantage for bent samples. Increasing the foot force (a heavier foot weight is supplied as standard) can lessen the effects on the Micro IRHD instrument.

Increasing the temperature by approximately 10°C appears to make a greater difference to IRHD results than Shore-M results, but the effect is small.

Repeated testing at the same location does make an appreciable difference to the results. This effect is more apparent when using the Shore-M instrument. This is important to realise when standard test blocks are used to check calibration.

The Shore-M result is relatively independent of foot force for a reasonable range of forces.

It is interesting to note that the results obtained from the Shore-M instrument with a dwell time of 3 seconds differ from those obtained using 1 second. Therefore, although the increased time used for comparative Shore-M tests is unimportant, it is important that the timing is accurate and repeatable.

Sample penetration is very much apparent in the case of a Shore-M Instrument whilst a Micro IRHD instrument is non-destructive and as such is suitable for testing end products. The disadvantage of the IRHD instrument is the time taken (35s specified by the standard). Previous work by Lackovic et al5 (1997) indicates that this time can be reduced by a predictive technique taking it into direct competition with the Shore-M timing, i.e. 3 seconds.

Conclusion

This paper has revealed many differences between the two instrument types. Both instruments clearly exhibit advantages in certain areas. For example, for testing samples of small dimensions, a micro IRHD instrument would be the preferred choice. The Shore-M test would be the preferred instrument for testing ‘bent’ samples. Other important considerations when selecting a test method have been covered. These include the awareness of the sample penetration using a Shore-M instrument which becomes important when repeatedly testing a sample or calibration block and during final product testing. The need for accurate and repeatable timing is important in the case of the Shore-M instrument to provide consistent results. Once the Shore-M instrument has an associated standard, the user can choose an instrument that best meets his needs.

Additional Work

Additional work needs to be carried out, investigating the testing of curved samples such as ‘O’ rings, where instrumental differences might be expected to have an effect.

References

  1. Briscoe, B. J. & Sebastian, K. S., ‘An Analysis of the “Durometer” Indentation’, Rubber Chemistry and Technology, Vol. 66, pp. 827-836, 1993
  2. Brown, R. P. & Soekarnein, A., ‘An Investigation of the Reproducibility of Rubber Hardness Tests’, Polymer Testing, Vol. 10, pp117-137, 1991
  3. ISO 48: 1994, Physical Testing of Rubber, Methods for the Determination of Hardness
  4. ASTM 1415-88 (1994), Test Method for Rubber Property – International Hardness
  5. Lackovic, S., Morgans, R. & McGarry, B., ‘Reducing the Duration of IRHD Hardness Tests’, International Conference on Rubbers, Calcutta, Dec. 1997

Download Paper 1 here.

]]>
Paper 2 – ‘Understanding the IRHD and Shore Methods used in Rubber Hardness Testing’ https://wallaceinstruments.com/paper-no-131-understanding-the-irhd-and-shore-methods-used-in-rubber-hardness-testing Mon, 08 Jun 2026 17:38:22 +0000 https://wallaceinstruments.com/?p=1320 Paper No. 2 – ‘Understanding the IRHD and Shore Methods used in Rubber Hardness Testing’ by R. Morgans1 * BSc, S. Lackovic2 BSc PhD, P. Cobbold 2

  1. University of Greenwich, School of Engineering, Medway Campus, Chatham Maritime, Kent ME4 4TB United Kingdom
  2. H W Wallace & Co Ltd, Curtis Road Industrial Estate, Curtis Road, Dorking RH4 1EJ United Kingdom

* Speaker

Presented at a meeting of the
Rubber Division, American Chemical Society
Orlando, Florida
September 21-24, 1999

Abstract

Hardness is one of the most widely measured properties used to characterise rubber

Two scales are in general use throughout the world – the IRHD (International Rubber Hardness Degree) scale and the Shore scale. The two test methods use totally different indenter geometries, applied forces, test times and procedures. Instruments exist for most of these scales – both as tabletop instruments and hand held versions – with little knowledge of the differences between them. National and international standards exist for most of these instruments; however, there are also some subtle differences between these standards. This paper looks at the instruments in question, studies the differences between the tests and their relationship between scales where possible. This paper also highlights the merits of each instrument and test type. In cases where measurements must be made on small or awkward production samples, the test method and sample dimensions may be highly significant and it is important to know the limitations of each test method. In conclusion, this paper aims to create a clear understanding of hardness testing methods and the results they provide.

Introduction

Hardness is one of the most widely measured properties used to characterise rubber. The IRHD (International Rubber Hardness Degree) Scale and the Shore Scale are widely used. A number of instrument types exist for both – the IRHD Micro/Dead Load and Shore A scales are most commonly used for rubber. Both methods are described in international standards.1, 2

The two test methods use totally different indenter geometries, applied forces, test times and procedures. The IRHD test is usually non-destructive, and as such has to be the preferred method for final product inspection; the test takes 35 seconds. In contrast, the Shore method is often destructive (leaving a permanent indentation), but the test only takes 1 or 3 seconds. The paper begins with a historical look at the instruments and the degree of correlation between them.

Instruments exist for most of the IRHD and Shore scales, both as tabletop and hand held versions. The IRHD Dead Load has a Micro counterpart, which has had an established standard for over 30 years (ISO 481 & ASTM 14152). The proposed Shore Micro does not yet have a released standard. The Micro IRHD instrument was introduced in the 1950’s as a scaled down version of the IRHD Dead Load – used for testing thinner, smaller samples and products. The Micro IRHD results are generally comparable to those given by the standard IRHD Dead Load instrument. In contrast there are various Shore M scale instruments appearing on the market; some constructed quite differently. The Shore M results are generally not comparable to those obtained from the Shore A scale.

Experience has shown that a degree of confusion exists between some users of the two scales. This paper highlights the merits of each instrument and test type. In cases where measurements must be made on small, awkward or curved production samples, the test methods and sample dimensions may be highly significant and it is important to know the limitations of each test method.

In summary, this paper aims to create a clear understanding of common hardness testing methods and the results they provide.

Historical perspective

According to Bassi et al3 the Shore instruments had historical priority over the IRHD instruments by more than 30 years. Gurney4 reported both instruments in use by the early 1920’s, together with other spring and dead load (weight) variants. Results from the spring type varied with the user (Gurney4, The Rubber Age5). This lead to the adoption of the dead load instrument where the indentation depth was largely user independent. After Scott6 stressed the need for a standard to give results some common meaning in 1935, the first British Standard (BS) was introduced in 1940. At the same time, Scott and Newton7 reported on a reliable pocket type hardness gauge that conformed to this new standard. After a comparison with the Shore A Durometer, they concluded that the advantage was always with the BS Hardness Meter. Work was then carried out looking at different instrument types (Daynes and Scott8) and the new standard (Scott9). They both agreed that there was some correlation between the Shore A and BS hardness scales.

The accuracy of a range of hardness testers (Newton10) was investigated, concluding that the main limitations were associated with the operator. Instruments with a spherical indenter and foot gave the smallest errors; the largest errors were associated with the Shore durometer. The largest source of variation reported by Scott11 was the lack of agreement between laboratories.

The Micro Hardness Tester, a (1/6th) scaled down version of the IRHD Dead Load Hardness Tester was introduced in the 1950’s to test thinner and small production samples. Scott and Soden12 reported results comparable between the Micro and Dead Load tests, with only a few degrees difference noted for rubbers of greater than 65° hardness.

Several papers3, 13, 14, 15 published in the 1960’s, 70’s and 80’s and two books, Rubber and Plastics Testing16 and Physical Testing of Rubbers17 stated that the most widely used instrument was then the Shore A type even though the IRHD method produced more repeatable results between operators, with higher accuracy, reproducibility and precision. However, Shore A has a less critical dependence than IRHD on sample thickness (Bassi et al3). Comparative work by Brown and Soekarnein18 (1991) between the IRHD Dead Load, IRHD Micro and Shore A instruments demonstrated that inter-laboratory repeatability was likely to be best for the IRHD Dead Load and Micro instruments. In 1993, Briscoe and Sebastian19 analysed the durometer indentation, providing an approximate relationship between IRHD and Shore A of (IRH » HA + 4), although this is very dependent on the sample compound.

Many contemporary hardness testers have improved accuracy due to the automatic nature of the test, requiring minimal operator intervention. Bench mounted instruments (IRHD Dead Load and Micro and Shore A scales) produce the most repeatable and reliable results. Pocket meters are much improved, but do rely entirely on the operator’s hand pressure and reliable angular application for repeatable results (variations can be extreme).

In recent years, there has been an increased interest in the Shore M instrument, although there is no published standard. There are a variety of these instruments on the market from several suppliers and some are constructed quite differently. Recently, Wallace has manufactured Shore M instruments to the best draft information available. The results are not comparable to those obtained from a Shore A instrument.

Differences between IRHD and Shore instruments and relationships between scales

There are four IRHD methods in use: the Normal-hardness test (Dead Load), High-hardness test, Low-hardness test and the Micro-test. The Normal test is used for samples greater than or equal to 4mm thick and preferably used for rubbers in the 35 to 85 IRHD range (but with reservation, may be used for the 30 to 95 IRHD range). The High-hardness test is used for testing samples of the same dimensions as the Normal test, but in the 85 to 100 IRHD range. The Low-hardness test is used for testing samples greater than or equal to 6mm thick and hardnesses in the 10 to 35 IRHD range. The Micro tests samples less than 4mm thick and is used for rubbers in the 35 to 85 IRHD range (but with reservation, may be used for the 30 to 95 IRHD range). All four methods use a spherically tipped indentor. The diameters of the ball indenter and foot vary between

methods. The applied forces are the same for the Normal, High and Low tests, with only the Micro test requiring the application of smaller forces. It is worth noting that the IRHD scale is non-linear.

The Shore range of hardness testers incorporates eight scale types: A, B, C, D, DO, O, OO and M. These are used for testing a wider range of materials. The A scale is used for soft rubbers and elastomers and type C for medium hard rubbers and plastics; both types use a truncated cone shaped indenter. Type A is the most commonly used rubber scale. Type B is used to test moderately hard rubbers and type D is used to test hard rubbers and plastics. Both of these use a 30° indenter. Type DO is used for very dense textile windings, type O is used for soft rubbers and medium density textiles and OO is used for low density textile windings and sponge. These three use a 3/32 inch spherically ended indenter. All types require samples more than 6mm thick (unless it can be proved that smaller samples give equivalent results). Type M (no published standard yet) is used for testing thin and irregular rubbers of hardness in the range 20 to 90 and uses a very small round tipped indenter. Thinner samples may be used, although the support table starts to affect the value as thickness falls as the indenter penetrates the sample. Spring forces vary between instruments. Type A, B and O use the same spring force and it is recommended that a force equivalent of 1kg is applied to the durometer to ensure that the spring force is repeatably overcome (note that the DIN standard uses 1.27kg and tighter indenter dimensional limits). Type C, D and DO use the same spring, requiring a force equivalent of 5kg to overcome the spring. Type OO uses a different spring and requires 400g. Type M currently suggests a force suitable to overcome the calibrated spring force. All Shore scales are linear.

The IRHD method is based on the use of dead loads (weights). A foot is used to hold the sample in place with a force of 8.3N (Dead Load) or 235mN in the case of the Micro hardness tester. A primary load of 0.3N (Dead Load) or 8.3mN (Micro hardness tester) is then applied for 5 seconds, providing a datum position. A secondary load of 5.4N (Dead Load) or 145mN (Micro) is then applied for 30 seconds. The incremental displacement from the datum is measured and converted to an IRHD value (a non-linear scale defined in the standard). The full-range displacement of (Normal) Dead Load is 1.8mm; the Micro uses 0.3mm.

In contrast, the Shore instruments use calibrated springs. For example, the Shore A scale spring force varies from 0.5N to 8.1N (over the full displacement) and the Shore M scale from 0.3N to 0.8N. The presser foot applies a force sufficient to overcome the spring force. Once the presser foot contacts the sample the indentation depth is recorded after a pre-set dwell time; the standard ASTM dwell times are 1 and 3 seconds. The DIN standard uses 3 seconds, since the reading is usually still changing appreciably after 1 second. The force increases linearly with indenter displacement (full range is 2.5mm for the A scale and 1.25mm for the M scale).

The IRHD scale was set in 1948 to correspond to the Shore scale, in that a high number indicates a hard rubber and a low number indicates a softer rubber. The original Micro hardness test was designed to be a scaled down version of the Normal Dead Load test (displacements in the ratio 6 to 1). The forces applied were in the ratio 36 to 1. Therefore if the limited thickness sample tested in the case of a Micro instrument is 1/6th of the thickness of the Dead Load piece, 1/6th of the result is obtained. Scaling is set so

that the same result should be obtained from both instruments. Similarly, results from the Normal, High and Low Dead Loads show correlation.

The Shore M test was not designed as a scaled down version of the Shore A test, but merely as an instrument that was capable of testing smaller samples. It uses an unrelated indenter and spring; there is no easy relationship between the two instruments.

Experimental

It follows from the above discussion that results obtained from hand-held durometers are not reliable due to operator dependence. Therefore, only bench mounted instruments were used to obtain the experimental results; however, the conclusions drawn will also be relevant to hand held instruments. Since the majority of rubber and elastomers use the Shore A and M scales, other Shore scales will be disregarded in this paper. These two instruments are also the main counterparts of the Normal and Micro IRHD instruments.

All instruments were calibrated before starting and the calibration was rechecked at the end. A standard temperature of 23±2°C was used (except where otherwise noted). The Shore instruments were set to both 1 and 3 second dwell time (since the results from these times differ). Test times are defined by the standard for the IRHD instruments (5 and 30 seconds). Each flat sample was tested in 5 different places and curved samples were tested as specified below.

A previous paper20 compared the Micro IRHD and Micro Shore instruments, looking at the effects of sample thickness, lateral dimensions, bent samples, temperature, re-testing a previously measure spot and the effect of the foot force on the Shore M instrument. The current paper aims to continue and extend this work to include the Dead Load and Shore A instruments as well as incorporating results from curved surfaces.

Standard Wallace test blocks (varying compounds of natural rubber, supplied by MRPRA) for both dead load and micro instruments were used to provide comparative results for each instrument.

The previous work20 on sample thickness was limited and therefore this is now investigated in further detail. The ISO standard1 allows 1mm thick samples to be used but the preferred thickness is 2 ± 0.5mm. It is known that Shore M has similar requirements. Tests were performed on a range of thinner materials. The Shore standard2 suggests that samples be plied to increase their effective thickness; this was done to determine the effect of varying sample thickness. This was extended to similar work on the IRHD dead load and Shore A instruments. The IRHD standard thickness is 8-10mm whilst the Shore A is 6mm. A selection of thinner samples were tested and plied to determine the effect of varying sample thickness.

Previous work20 with the Micro instruments included an investigation into the effect of increasing the ambient temperature. Therefore tests were carried out on the Dead Load and Shore A instruments at a raised temperature to determine any effect.

Curved samples, such as ‘O’ rings, are often tested and the effect of testing these on different instruments was investigated. ‘O’ rings (of varying outer and core diameters) were placed on a specially designed table so that they could be accurately displaced laterally to determine the effect of testing away from the top dead centre.

Results

Standard Test Blocks

The standard test blocks gave repeatable results using Micro and Normal Dead Load instruments. The 1 and 3 second dwell times (Shore A and M) produced equivalent and repeatable results. The Dead Load readings were consistently a few units higher than the Shore A readings over the range tested (40 – 90 IRHD). However, there was an increasing tendency for the Shore M results to diverge from the Micro IRHD result with increasing hardness values.

Effects of Thickness

The IRHD Dead Load and Shore A instruments were used to test the standard Wallace Micro samples (2mm thick). As expected, the results differed from those obtained using the specified instrument for the sample thickness, i.e. the Micro IRHD and the Shore M types. The softer rubbers, and also the IRHD Dead Load instrument, exhibited greater differences between the micro and macro instrument results. For the hardest rubber (76-79 IRHD), the IRHD Dead Load instrument gave a very close value (see figure 1). The Shore A instrument read a few units lower as expected but the readings were closer between the Shore A and Shore M instruments. The Shore A value of the hardest rubber differed by only 1 unit to the Shore M value (figure 1).

Figure 1 – Testing 2mm thick samples on micro & macro instruments

Figure 2 - Decreasing hardness with increasing sample thickness

Once the 2 mm thick samples were plied to 8mm thick (the standard thickness required for the IRHD Dead Load tester) the results came within the specified tolerances of the test pieces. Increasing the thickness further made little difference to the result. Using the Shore A instrument, the results after plying pieces to provide a 6mm thick sample (the standard thickness for Shore A) was not equivalent to the value when tested with a Shore M instrument. See figure 2.

Figure 2 – Decreasing hardness with increasing sample thickness

In contrast, the standard Dead Load blocks of 8mm thick, when tested on the Micro IRHD and the Shore M instruments, tended to give approximately the same results as the Dead Load IRHD and Shore A instruments.

Various thinner samples were used with the micro instruments. Up to 5 pieces of neoprene (0.6mm thickness) were plied, taking the thickness of the sample into the standard tolerance region (and slightly beyond). Both the IRHD Micro and Shore Micro showed a continual decrease in hardness with increasing thickness (see figure 3). As before, the IRHD hardness values were consistently higher than the Shore M values. For a nitrile sample, the readings at the initial thickness of 1.5mm (within the tolerance given in the standard) were similar between instruments. The Shore M results remained constant during the thickness increase but the IRHD Micro instrument showed a decrease in hardness with increasing thickness to 4.5mm. In the case of a sample of silicone, the Shore M results were consistently lower than the IRHD Micro values, but both instruments exhibited a decrease in hardness of 1 unit, when doubling the thickness of the sample from 0.9mm to 1.8mm (within the standard).

Figure 3 - Increasing the thickness of a neoprene sample

Figure 3 – Increasing the thickness of a neoprene sample

Effect of Temperature

Raising the temperature by 10°C appeared to make little difference to the results from the IRHD Dead Load on the standard test blocks (natural rubber compound). However, slightly lower values were observed on the harder samples tested on the Shore A instrument.

Effect of Curved Surfaces

The smaller diameter ‘O’ rings were laterally displaced in increments of 0.25mm. The larger curved surfaces were displaced in increments of 0.5mm. Graphs were plotted, showing the change in apparent hardness as the sample was displaced across the indenter. In general, the resulting curves on the graphs were flatter when testing the ‘O’ Rings on a Micro IRHD instrument than on the Shore M instrument. The Shore M instrument produced curves which were more peaked, with the hardness values rapidly decreasing on either side of top dead centre (figure 4).

A piece of pipe (8mm diameter) was tested on the IRHD Dead Load and Shore A instruments; both gave fairly flat curves. An EPDM O- ring of core diameter 7.8mm produced a gentle curve when tested on the Shore A instrument, but when tested on the IRHD Dead Load, it was inverted.

Discussion

From the results it is clear that there is a correlation between the Dead Load and the Micro IRHD instruments. This is apparent when the IRHD Dead Load result of plied micro samples corresponds with the standard result on an IRHD Micro instrument. In contrast, the same cannot be said for the Shore A and M scales.

The results indicate that the thickness of the sample used on the IRHD Dead Load affects the result more than on the Shore A, in agreement with Bassi et al3.

In general, when the nitrile, neoprene and silicone samples were plied, a trend of decreasing hardness with increasing thickness was observed. Some differences were noted and it appears that different rubber types influence the results in slightly different ways. More extensive work is required in this area.

Generally, the micro instruments can be used for testing both micro and macro samples, whilst the macro instruments (IRHD Dead Load and Shore A) are better for macro samples. Indeed, many people now use the Micro IRHD instead of the Dead Load instrument.

Flatter curves are produced with the IRHD Dead Load, Micro and the Shore A instruments when testing curved samples, implying that there is less critical dependence on accurate sample positioning with these. Since the graphs produced when using the Shore M instrument are more peaked, it is important to accurately place the sample (to within ~ 0.1mm). However, this is controlled when using an instrument attachment to centralize ‘O’ rings, but remains important when testing curved shapes that cannot be held accurately in such an attachment.

Increasing the temperature by approximately 10°C appears to make a greater difference to harder natural rubber samples only on the Shore A and little difference using the IRHD Dead Load instrument. This compares to a slight effect noted in the previous work20 with both the IRHD Micro and the Shore M instruments.

From previous work, it is clear that repeated testing at the same location makes an appreciable difference to the results. This is more apparent when using the Shore M instrument. It is important to ensure that the sample is displaced between tests – this can be difficult for small samples.

It is interesting to note that the results obtained from the Shore instruments with a dwell time of 3 seconds differ from those obtained using 1 second. This effect was demonstrated more effectively in previous work20. Therefore, for Shore instruments, although different timings are unimportant for comparative work, it is important that the timing is accurate and repeatable. The time required (35 seconds specified by the standard) for an IRHD test places the IRHD instruments at a disadvantage. However, previous work by Lackovic et al21 indicates that this time can be reduced by a predictive technique, taking it into direct competition with the Shore timing, i.e. 3 seconds.

Conclusion

This paper has taken a historical look at the IRHD and Shore Hardness measurement instruments as well as discussing and emphasising the fundamental differences between the most common instruments used for rubber and elastomer hardness characterisation. As demonstrated in a previous paper20, the various instruments exhibit advantages and disadvantages with certain sample types. IRHD instruments are preferred for non-destructive testing and the Micro IRHD is generally a better choice for testing curved surfaces. The Shore A instrument is preferable for testing non-standard thickness samples and when shorter test cycle times are required. Accurate and repeatable timing is critical to allow Shore A and M instruments to provide consistent and comparable results.

References


1. ISO 48: 1994, Physical Testing of Rubber, Methods for the Determination of Hardness
2. ASTM 1415-88 (1994), Test Method for Rubber Property – International Hardness
3. A. C. Bassi, F. Casa & R. Mendici, Polymer Testing 7, 165 (1987)
4. H. P. Gurney, India Rubber Journal 497 (1921)
5. ‘A New Rubber Hardness Tester’, The Rubber Age 29, 242 (1939-40)
6. J. R. Scott, Transactions I. R. I. 11, 224 (1935)
7. J. R. Scott & R. G. Newton, Journal of Rubber Research 9, 91 (1940)
8. H. A. Daynes & J. R. Scott, Journal of Rubber Research 12, 94 (1943)
9. J. R. Scott, Journal of Rubber Research 17, 145 (1948)
10. R. G. Newton, Journal of Rubber Research 17, 178 (1948)
11. J. R. Scott, Transactions I. R. I. 27 (5), 249 (1951)
12. J. R. Scott & A. L. Soden, Proceedings of the International Rubber Conference, Washington, Paper 22, pp. 170-176 (1959)
13. K. Price, Progress of Rubber Technology 42, 59 (1979)
14. J. C. Warner & J. A. Jerdonek, European Rubber Journal & Urethanes Today 162, 11 (1980)
15. W. V. Chang & S. C. Sun, Rubber Chemistry and Technology 64, 202 (1991)
16. “Rubber and Plastics Testing”, Klucklow, pp. 153-162, 1963
17. “Physical Testing of Rubbers”, J. R. Scott, pp. 91-110, 1965
18. R. P. Brown & A. Soekarnein, Polymer Testing 10, 117 (1991)
19. B. J. Briscoe & K. S. Sebastian, Rubber Chemistry and Technology 66, 827 (1993)
20. R. Morgans, S. Lackovic & P. Cobbold, The International Rubber Exhibition & Conference Book of Papers, Manchester, UK,
Materials Paper 12 (1999)
21. S. Lackovic, R. Morgans & B. McGarry, The International Conference on Rubbers, Calcutta, India, Paper AT-5 (1997)

Download Paper

]]>
Compression Stress Relaxation – Understanding Long Term Performance Under Compression https://wallaceinstruments.com/compression-stress-relaxation-understanding-long-term-performance-under-compression Mon, 08 Jun 2026 16:20:03 +0000 https://wallaceinstruments.com/?p=1305 Compression Stress Relaxation – Understanding Long Term Performance Under Compression

What you will learn

Everything you need to know about compression stress relaxation testing – why it’s important, what it measures, how the test works, and how to get reliable results.

Rubber components under compression

Rubber and elastomeric components are found in countless engineered products across automotive, aerospace, oil and gas, medical, construction, consumer electronics and industrial manufacturing sectors. They function as seals and gaskets, vibration isolation mounts, structural bearing pads, cushioning components and more. In many applications, a component that degrades or loses its properties is an inconvenience. In others it is a safety event, where the integrity of the system depends on the rubber maintaining its counterforce reliably over years or decades of service.

What makes this degradation particularly difficult to manage is that it rarely happens suddenly. It happens gradually, as the rubber relaxes under compression and the force it exerts against the mating surfaces diminishes over time. The component may look perfectly intact, yet the counterforce begins to decay from the moment it is installed. Initially this is driven primarily by physical relaxation within the polymer network, while over longer timescales chemical degradation mechanisms such as chain scission, thermo-oxidative ageing and changes to the crosslink structure increasingly contribute to the loss of force. The rate of decay is influenced by temperature, chemical exposure, time and the formulation of the elastomer itself.

Understanding how that counterforce decays over time – measuring it, predicting it, and using it to select the right material for the application – is exactly what compression stress relaxation (CSR) testing is designed to do.

What is compression stress relaxation?

When a rubber component is compressed between two rigid surfaces and held at a fixed deformation, the force it exerts against those surfaces does not remain constant. It decreases with time. This phenomenon is compression stress relaxation – the gradual reduction in counterforce exerted by a rubber material held under constant compressive strain.

It is important to be clear about what is actually happening. The deformation is fixed – the gap between the two surfaces does not change. What changes is the force the rubber exerts against them. In a sealing application, that force is the sealing force. As it decays, the seal becomes progressively less effective, even though it has not physically moved or visibly deteriorated.

Two distinct mechanisms drive this decay. The first is physical relaxation – the rearrangement of the polymer network under sustained deformation. This occurs relatively quickly and is largely reversible if the stress is removed. The second is chemical relaxation – irreversible changes to the polymer network through chain scission, thermo-oxidative degradation, or changes to the crosslink structure. These processes are temperature-dependent and become increasingly dominant over longer timescales and at elevated temperatures.

In practice both mechanisms occur simultaneously. The relative contribution of each depends on the rubber compound, the temperature, and the duration of the test or service period. Polymer type, crosslink system, filler package and antioxidant selection can all significantly influence compression stress relaxation performance. Because rubber properties are highly temperature dependent, and because rubber and steel have significantly different coefficients of thermal expansion, even small temperature fluctuations during a CSR test can introduce measurement error – a challenge inherent to the test method itself rather than to any specific instrument. The two main test methods defined in the governing standards – Method A and Method B – offer different approaches to managing this challenge, as discussed in the standards section.

CSR versus compression set

Compression set and compression stress relaxation both involve compressing a rubber sample between two rigid surfaces, but they measure fundamentally different things.

Compression set is a simple end-point measurement. A sample is compressed by a defined amount for a fixed time at a fixed temperature, then released. The test measures how much permanent deformation remains after the stress is removed – a useful indication of elastic recovery, but one that tells you nothing about what happened to the counterforce during the compression period itself.

CSR does exactly that. The sample remains compressed throughout the test and the force it exerts against the compression plates is measured at defined intervals. The result is a picture of how counterforce decays over time under sustained compression – a much closer simulation of what actually happens in service. A material can show acceptable compression set results and still exhibit rapid force decay under sustained compression, which is why the two tests are not interchangeable in specifications where long-term performance under compression is critical.

Where CSR testing is used

CSR testing is used wherever the long-term performance of a rubber or elastomeric component under sustained compression is critical to safety, reliability or product warranty.

In automotive engineering, engine seals, gaskets and other elastomeric components are subject to sustained compression over long service intervals under demanding thermal and chemical conditions. CSR testing is well established in automotive material specifications, particularly for sealing applications expected to maintain performance over long service intervals.

In aerospace, engine seals, hydraulic system seals and fuel system components must retain sealing force reliably across wide temperature ranges over the operational life of the aircraft. CSR data is commonly used during material qualification and evaluation of aerospace elastomers.

In construction and infrastructure, elastomeric pipe joint seals, bridge bearing pads and building facade gaskets are subject to sustained compression over service lives measured in decades. Long-term sealing force retention is essential to system integrity in applications where access for inspection or replacement is limited.

In oil and gas, seals and gaskets in subsea and downhole applications may be inaccessible for years or decades. CSR testing forms part of the compound qualification and material selection process for these applications, where getting the material right before installation is the only option.

Beyond sealing applications, CSR testing is also widely used in compound development and material evaluation, characterising how different elastomer formulations behave under sustained compression, comparing compounds, and understanding degradation mechanisms. It can also be applied to elastomeric components where retention of compressive force is important to long-term performance, including vibration isolation mounts, structural bearing pads and cushioning components.

Wallace and CSR – a long history

Wallace’s involvement in compression stress relaxation testing goes back to 1981, when a paper published in the journal Polymer Testing, co-authored by H. W. Wallace & Co. Ltd and the Rubber and Plastics Research Association (RAPRA) at Shawbury, described the development of a new compression stress relaxation jig designed to overcome the limitations of existing designs. The key innovation was a parallel spring diaphragm system that achieved high lateral stability without friction – addressing one of the fundamental practical challenges of accurate CSR measurement.

That jig – the Shawbury-Wallace fixture – remains in production today and is one of only two jig designs specifically illustrated in ASTM D6147-97(2020), the current American standard for compression stress relaxation testing. The Wykeham Farrance fixture is the other. Wallace supplies both, giving customers the choice of either established design, fully compatible with the WAC11 Mk5.

Over more than four decades since that original paper, Wallace has continued to develop its CSR capability. The WAC11 Mk5 represents the current generation of that work.

The Wallace WAC11 Mk5

The Wallace WAC11 Compression Stress Relaxometer Mk5 is designed to make CSR testing straightforward, accurate and efficient – whether in a quality control laboratory running routine tests on incoming seal materials or in an R&D environment developing new elastomeric compounds for demanding applications.

The instrument operates on the discontinuous measurement principle. The test sample is compressed by a known amount in a Wallace jig, and the jigs are stored at the required test temperature – in an oven or at ambient conditions – between measurements. At each measurement interval, the jig is brought to the WAC11 and the instrument measures the counterforce exerted by the test sample. The measurement principle is based on an electrical contact between the load cell and the head of the jig, which is broken only when the force applied by the WAC11 marginally exceeds the counterforce of the test sample. This approach ensures that the over-compression applied during measurement is kept to a minimum, as required by the standards.

The measuring head is ballscrew-driven and motorised. It approaches the jig quickly to save time, then slows to a controlled speed before contact to allow the load cell to read the force accurately. When the contact opens, the counterforce is recorded, displayed graphically and saved automatically.

The software collects counterforce data from multiple jigs simultaneously, allowing any number of jigs to be managed with a single instrument. Tests can be designed and customised to suit specific requirements, with almost unlimited flexibility in test parameters, measurement intervals and reporting formats. Results are stored and can be exported via USB or network ports.

A key practical advantage of the WAC11 Mk5 is its backwards compatibility. It accepts jigs from previous Wallace models as well as industry-standard Shawbury-Wallace and Wykeham Farrance jig designs, including tooling from other manufacturers. Customers who have already invested in jigs and fixtures are not forced to replace them when upgrading their instrument.

Note that the Wykeham Farrance jig is limited to 13mm diameter samples; the Shawbury-Wallace accommodates all sample sizes specified in both ISO 3384-1 and ASTM D6147.

The WAC11 Mk5 does not require a separate tensometer to operate. For laboratories where tensometer capacity is limited or where CSR tests run over long periods, this is a meaningful operational advantage.

Test specimens and jigs

Test specimens

CSR test specimens are cylindrical discs or rings prepared from moulded or sheet rubber. The standard disc dimensions specified in ISO 3384-1 and ASTM D6147 are 13 mm diameter by 6.3 mm thick, or 29 mm diameter by 12.5 mm thick. Ring test pieces are particularly suited to liquid immersion testing – for these applications, the compressed jig is immersed in the test fluid between measurements rather than stored in an air oven, and the drilled jig plates allow the fluid to access both the inner and outer surfaces of the ring specimen. The preferred compression level in both standards is 25 ±1%, with 15 ±1% permitted where 25% cannot be achieved.

Jigs

Wallace supplies two jig designs for use with the WAC11, both referenced in ASTM D6147. The Shawbury-Wallace jig is available in fixed-height (C11/1) and adjustable (C11/6) variants, accommodating a wide range of sample thicknesses and compression percentages, with bespoke spacers available for non-standard applications. An O-ring adaptor (C11/7) is available for both variants, accommodating O-rings of up to 41 mm diameter with a venting hole to prevent pressure differential across the seal during testing. The Wykeham Farrance jig is a fixed-height design limited to 13 mm diameter samples. All jig assemblies are manufactured from stainless steel as standard, with alternative materials available for specific chemical environments, and both designs operate across a temperature range of -40°C to +250°C.

Using CSR data for service life prediction

One of the most valuable applications of CSR testing goes beyond quality control and incoming material inspection. When conducted systematically across a range of temperatures, CSR data can be used to predict the service life of an elastomeric component – estimating how long a material will continue to provide effective counterforce under real-world operating conditions.

CSR results are typically expressed as the percentage of the original compressive force retained after a given period, or as the percentage loss in force over time. Plotting force retention against time provides a useful way to compare compounds, assess degradation behaviour and evaluate long-term performance under sustained compression. The resulting force retention curves form the basis for many material selection and service life prediction studies.

The approach is based on the Arrhenius equation, which describes how the rate of chemical reactions – including the degradation processes that drive long-term CSR – increases with temperature. By running CSR tests at several elevated temperatures and measuring the time taken for the counterforce to reach a defined end-of-life threshold, it is possible to construct an Arrhenius plot. This plots the logarithm of the time to reach the threshold against the inverse of the test temperature in Kelvin. A line drawn through the data points can then be extrapolated to the actual service temperature, giving an estimate of the time required to reach the defined end-of-life criterion. The principles and procedures for this methodology are set out in ISO 11346:2023.

This approach is particularly valuable for applications where direct long-term testing at service temperature would take years. By testing at elevated temperatures over a shorter period, service life at lower temperatures can be estimated with reasonable confidence.

There are important caveats. The Arrhenius approach assumes that the same degradation mechanism dominates across all test temperatures, which is not always the case – some rubber compounds show non-Arrhenius behaviour at certain temperature ranges. Results should be interpreted with appropriate caution, particularly when extrapolating over very long timescales or to temperatures significantly below the lowest test temperature. ISO 11346:2023 provides guidance on the correct application of the method and its limitations.

Governing standards

CSR testing of rubber and elastomeric materials is governed by three main standards, all of which the Wallace WAC11 Mk5 is designed to meet using Method B where applicable.

ISO 3384-1:2024 is the primary international standard for compression stress relaxation testing at constant temperature, adopted in the UK as BS ISO 3384-1:2024. It specifies two procedures – Method A, in which compression and all force measurements are made at the test temperature, and Method B, in which compression and all force measurements are made at standard laboratory temperature with the jigs stored at the test temperature between measurements. The WAC11 operates to Method B. The two methods can produce different results because of the way measurements are made, and data generated using one method should not normally be compared directly with data from the other.

ISO 3384-2:2019 covers stress relaxation testing with temperature cycling, where the test piece is subjected to alternating high and low temperatures rather than a single constant test temperature, adopted in the UK as BS ISO 3384-2:2019. This is particularly relevant for automotive and aerospace applications where components experience significant temperature excursions in service.

ASTM D6147-97(2020) is the American standard for compression stress relaxation testing, specifying two methods for determining the decrease in counterforce exerted by a rubber or thermoplastic elastomer test piece under constant compression. The WAC11 supports Method B only. Results generated in accordance with ASTM D6147 and ISO 3384-1 should not be assumed to be directly comparable, as the standards differ in their procedures, measurement approaches and reporting requirements.

Wallace – your partner in CSR testing

Compressive force retention is a practical engineering problem with real consequences – for safety, for reliability, for warranty and for the people and systems that depend on elastomeric components performing as specified, year after year.

Compression stress relaxation testing exists because a single end-point measurement is not enough. Understanding how counterforce decays over time – under heat, under sustained compression, in challenging chemical environments – requires a test that reflects the reality of service conditions as closely as possible.

Wallace has been part of that story since the early days of standardised CSR testing. The Shawbury-Wallace jig, developed in collaboration with leading researchers in the field and referenced by name in ASTM D6147 more than four decades on, is a measure of the enduring influence of that original engineering contribution. The WAC11 Mk5 represents the current generation of that work.

If you have questions about CSR testing, instrument selection, jig specification or calibration, the Wallace technical team is happy to help. Get in touch.

]]>
What is PRI Testing? https://wallaceinstruments.com/what-is-pri-testing Wed, 20 May 2026 09:17:33 +0000 https://wallaceinstruments.com/?p=872 What is PRI Testing?

A quality standard at the heart of global natural rubber supply

What you will learn

Everything you need to know about the Plasticity Retention Index – what it measures, why it matters in the natural rubber supply chain, and how to get consistently reliable results.

Natural rubber – a global commodity

Natural rubber remains one of the world’s most strategically important industrial materials. Derived from the latex of the Hevea brasiliensis tree, it is used in the manufacture of tyres and a vast range of other products across industrial, medical and consumer sectors – valued for a combination of high elasticity, resilience and tear resistance that remains difficult to replicate in synthetic alternatives for many critical applications.

The rubber tree’s origins are in South America, but the majority of the world’s natural rubber is grown in Southeast Asia, with Thailand, Indonesia and Vietnam the three largest producers. West Africa is a rapidly growing presence, with Côte d’Ivoire an increasingly significant supplier. The rubber tree cannot be commercially cultivated outside the tropical band – it requires heat, humidity and well-distributed rainfall – which means the global supply chain remains geographically concentrated and subject to the climatic, agronomic and geopolitical conditions of a relatively small number of producing countries.

The challenge of consistency and the TSR scheme

Natural rubber is not a manufactured material with a controlled composition – it is an agricultural product, and like all agricultural products it varies. Tapping takes place early in the morning, typically before dawn, when the tree’s internal pressure is at its highest and latex flow is greatest. A shallow diagonal cut is made in the bark using a specialised tapping knife, channelling latex into collection cups below. The tapped latex consists of around 30 to 35% rubber hydrocarbon, with the remainder made up of water, proteins, fatty acids, amino acids, starches, sterols and various other non-rubber constituents. A rubber tree reaches maturity and begins producing latex at around five to seven years, and a well-managed tree can remain productive for 25 to 30 years.

Natural rubber is produced by both large industrial plantations and smallholder farmers, and this has important implications for consistency. On larger plantations, fresh latex is collected daily and taken to an on-site processing facility. Depending on the intended market, it may be concentrated and exported as liquid latex, sheeted and smoke-dried to produce ribbed smoked sheet, or coagulated with acid, washed, milled and dried in hot-air tunnel ovens to produce block rubber, pressed into 33.3 kg bales. Smallholder material can follow a less controlled path – latex is often allowed to coagulate naturally in the collection cups over several days before being collected, resulting in what is known as cup lump. This material is gathered and sold to local dealers or processing centres for bulking and processing.

The processing route matters because it directly affects quality – and so does the natural variability of the rubber itself. The levels of naturally occurring antioxidants vary between tree clones and change as the tree matures, significantly influencing how the rubber ages and degrades in processing and in service. Managing this variability has been one of the central challenges of the natural rubber supply chain.

The introduction of Technically Specified Rubber (TSR) grading brought consistency and objectivity to the rubber trade, establishing for the first time a system in which natural rubber was graded on the basis of measured technical specifications rather than visual appearance. Malaysia led the way, launching the Standard Malaysian Rubber (SMR) scheme in 1965. Other major producing nations followed with their own equivalent schemes, with ISO subsequently developing international standards to underpin and harmonise the approach. Each country now has its own national designation within the TSR framework – Thailand uses STR (Standard Thai Rubber), Indonesia uses SIR (Standard Indonesian Rubber), Malaysia uses SMR, and India uses ISNR (Indian Standard Natural Rubber). Despite the different names, the underlying technical requirements across equivalent grades are the same, governed by ISO 2000.

What is PRI and what does it measure?

The Plasticity Retention Index (PRI) is one of the key parameters in the TSR grading system. Together with dirt content, ash content, nitrogen content, volatile matter, initial plasticity (P₀) and Mooney viscosity (plus some additional parameters that only apply to specific grades), these measured properties give everyone in the supply chain an objective, guaranteed picture of the material they are purchasing.

PRI measures how well natural rubber resists thermal oxidative degradation – in plain terms, how well it holds up when exposed to heat and oxygen. It is expressed as a ratio of aged to unaged plasticity, and while it does not provide an absolute measure of oxidative stability, the TSR grading system sets minimum thresholds for that ratio by grade. It is used for grading technically specified rubbers across the natural rubber supply chain – from plantations and processing centres through to incoming QC at tyre manufacturers and other rubber product producers.

Under ISO 2000:2020, TSR 20 requires a minimum PRI of 40, TSR 10 a minimum of 50, and higher grades including TSR L, TSR WF, TSR 5 and CV grades a minimum of 60. Reliable PRI data is essential to predictable processing behaviour and end-product performance – and it is against that backdrop that PRI testing takes on its full significance.

PRI is calculated by comparing plasticity before and after ageing, using a straightforward ratio:

PRI = (Median P₃₀ / Median P₀) × 100

P₀ is the median plasticity of three unaged test specimens. P₃₀ is the median plasticity of three matched specimens after ageing for 30 minutes at 140°C. The ratio, expressed as a percentage, shows how much of the original plasticity is retained after that controlled ageing cycle.

A high PRI value indicates strong resistance to thermal oxidative degradation. The rubber retains most of its plasticity after ageing, which in practice means it will process more predictably and consistently. A low PRI indicates that greater degradation has occurred during ageing, which may affect mill behaviour, compound processing characteristics and ultimately the properties of the finished product.

How PRI testing works – an overview

PRI testing is a multi-step process that requires careful control at every stage. Raw rubber is prepared and cut into disc-shaped test pieces, which are divided into two matched sets. One set is aged in an oven at 140°C for 30 minutes while the other remains unaged. After ageing and cooling, both sets are tested on a parallel-plate plastimeter within a defined time window. The median plasticity values from each set give P0 and P30, from which the PRI is calculated.

Throughout the process, accurate sample matching and strict timing are essential to the integrity of the result.

The Wallace integrated PRI testing system

Achieving consistent, reliable PRI results depends not just on the quality of individual instruments but on how well the entire workflow is controlled from start to finish. The P14 Rapid Plastimeter, WAO14 Ageing Chamber, S2 Volumetric Specimen Cutter, traceability fixture and software are designed as an integrated system – each specified to work with the others to deliver standards-compliant results with minimal operator influence.

S2 Volumetric Specimen Cutter cuts up to 30 uniform disc specimens per minute, ensuring consistent sample geometry and removing one of the key variables in the preparation stage.

Wallace WAS4-14 Thickness Gauge is used to verify that each test piece is within the required thickness tolerance before testing proceeds, ensuring sample consistency from the outset.

WAO14 Ageing Chamber is available in two capacities, the O14-48 and O14-96, controlling temperature to ±0.2°C, exceeding the ±0.5°C requirement of ISO 2930:2024. Individually timed drawers and rapid thermal recovery after sample loading support consistent, reproducible ageing conditions.

O14 Traceability Fixture is available in 48 and 96-sample capacities to match the respective oven models. Colour-coded tabs make it simple to match aged and unaged specimens at every stage, reducing handling errors and keeping the workflow organised even at high sample volumes.

P14 Rapid Plastimeter Mk V is the central instrument for measuring plasticity. The P14 applies a precisely controlled load to the test piece and measures the resulting deformation, expressed in Rapid Plasticity Units where one unit equals 0.01 mm. Automated timing of both compression phases eliminates operator variability at one of the most critical points in the test.

Traceability software connects multiple instruments to a single server for centralised data management, with configurable data fields to meet the reporting and traceability requirements of individual laboratories and quality management systems.

As with all Wallace instruments, the PRI system is designed with the busy laboratory environment in mind. Each instrument has a compact footprint, a clean and considered design, and an intuitive interface – making efficient use of bench space without compromising on capability, supporting Wallace’s four core principles – Productivity, Reliability, Repeatability and Traceability – across every step of the PRI testing process.

Sample preparation

Correct sample preparation is essential to the validity of PRI results. The raw rubber is first homogenised in accordance with ISO 1795 using a laboratory mixing mill at 27 ±3°C and sheeted to the correct thickness. Six disc-shaped test pieces are then cut from the prepared sheet using the Wallace S2 Volumetric Specimen Cutter, and each is checked with the Wallace WAS4-14 Thickness Gauge to confirm it is within the required thickness tolerance. The six specimens are divided into two matched sets of three – one set for ageing, one to remain unaged – with the Wallace O14 Traceability Fixture keeping the two sets clearly identified and organised throughout.

The testing process

Ageing the samples

The three specimens designated for ageing are placed on aluminium dishes in the Wallace WAO14 Ageing Chamber, which must be stable at 140°C before samples are loaded. The required ageing period is 30 minutes. The WAO14 controls temperature to ±0.2°C – exceeding the ±0.5°C requirement of ISO 2930:2024 – and its individually timed drawers allow multiple batches to be managed simultaneously without confusion. According to Wallace instrument specifications, temperature should recover to within 1°C of the set point within 5 minutes of sample insertion. After removal, samples are allowed to cool to room temperature.

There is a critical timing requirement: plasticity testing must be carried out no earlier than 30 minutes and no later than 2 hours after the end of ageing. The aged and unaged measurements must be made within the same session, using the same instrument and the same type of paper throughout. Testing outside this window will give unreliable results.

Matching samples

Aged and unaged specimens must be correctly matched before testing. The Wallace O14 Traceability Fixture colour-coded tabs identify which aged specimen corresponds to which unaged specimen, eliminating the risk of matching errors even when processing high volumes of samples simultaneously.

Running the plasticity test

Aged and unaged measurements must be made concurrently using the same type of paper throughout. Place each specimen between two pieces of tissue paper as specified in ISO 2930:2024 and position centrally between the heated platens of the Wallace P14 Rapid Plastimeter, maintained at 100°C.

Each specimen is enclosed between two pieces of tissue paper as specified in ISO 2930:2024 and positioned centrally between the heated platens of the Wallace P14 Rapid Plastimeter, maintained at 100°C. An initial clamping force of at least 300 N is applied for 15 seconds, compressing the sample to a defined thickness of 1 mm and pre-heating it. A measuring force of 100 N ±1 N is then applied for a further 15 seconds, and the reduction in thickness at the end of this period is measured and expressed in Rapid Plasticity Units, where one unit equals 0.01 mm. The automated timing of both compression phases eliminates operator variability at one of the most critical points in the test. The median of the three readings from each set gives P₀ for the unaged specimens and P₃₀ for the aged specimens, from which the PRI is calculated.

Factors that affect your results

Even with the correct equipment in place, three variables most commonly introduce error in PRI testing and are worth understanding in detail.

Platen load. The standard specifies a measuring force of 100 ±1 N. Even within the permitted tolerance, load variation has a measurable effect – a load of 97 N will increase the plasticity result by approximately 1.5 units relative to the nominal 100 N load, and a load of 103 N will decrease it by a similar amount. The Wallace P14 applies load via a calibrated weight arm, ensuring consistent, repeatable force with every test.

Sample positioning. The sample should be placed at the centre of the lower platen. Minor deviations of a few millimetres have no measurable effect, but once the upper platen edge contacts the sample – typically from about 5 mm off-centre – the plasticity number drops by approximately 1 unit and continues to fall as less of the sample is evenly compressed.

Platen parallelism. Non-parallel platens introduce systematic error, and the effect is amplified when using alternative platen sizes, which the standard permits for harder or softer rubbers and silicones. Parallelism must be checked and reset every time the platen is changed.

Reporting requirements

A compliant test report under ISO 2930:2024 should include the following:

the full description and identification of the sample including its origin; the milling procedure used in sample preparation with reference to ISO 1795; the testing method with reference to ISO 2930:2024; details of the instruments used; the platen size and test temperature; the plasticity numbers P₀ and P₃₀ and the calculated PRI value rounded to the nearest whole number; and the date of testing.

The Wallace P14 traceability software captures test data automatically – eliminating transcription errors and providing a clear, auditable record for every test. Configurable data fields allow laboratories to capture additional sample and batch information to meet the requirements of individual customers or quality management systems. For laboratories operating under ISO 17025 or supplying into quality-critical industries such as tyre manufacturing, this level of traceability is increasingly expected as standard.

Governing standards

ISO 2930:2024 is the current international standard for PRI testing, now in its sixth edition. It specifies the method for determining the plasticity retention index of raw natural rubber, covering sample preparation, ageing conditions, plasticity measurement and reporting requirements. First published in 1974, it has been revised several times, reflecting its ongoing central importance to the natural rubber industry.

ASTM D3194 is the American equivalent. While the underlying PRI calculation is identical, there are meaningful differences in sample preparation – including milling temperatures (70 ±5°C under ASTM versus 27 ±3°C under ISO), sample portion sizes, and test paper specification – which mean results obtained under the two standards are not directly comparable. Laboratories supplying into both international and American markets need to be clear about which standard applies to each customer or specification requirement.

ISO 2007:2018 specifies the rapid plastimeter method for measuring plasticity of unvulcanised rubber – the test method referenced within ISO 2930 for both the P₀ and P₃₀ measurements. It covers not just PRI testing but the broader application of plasticity measurement to raw and unvulcanised compounded rubber.

ISO 1795:2017 specifies sampling and further preparative procedures for raw natural and synthetic rubber, referenced within ISO 2930 for the homogenisation and sample sheet preparation steps.

ISO 2000:2020 provides guidelines for the specification of TSR grades, including the minimum PRI values required for each grade. This is the standard that links PRI testing directly to the commercial grading and trading of natural rubber, and within which Wallace instruments and the PRI test method play a central role.

PRI testing – precision in a natural product

Natural rubber begins its journey in a tropical plantation, tapped by hand before dawn, processed and traded across the globe before it reaches a compounder’s mill. At every stage, variability is inherent – in the tree, in the clone, in the processing route, in the conditions of storage and transport.

PRI testing exists because that variability matters. A single number – the ratio of aged to unaged plasticity, expressed as a percentage – gives buyers, processors and quality teams a reliable, objective indication of how a batch of natural rubber will behave. It is a key parameter in the grading system that has brought consistency and trust to the natural rubber supply chain since the 1960s.

Getting that number right demands more than good instruments. It demands a controlled, repeatable workflow from the moment the sample is prepared to the moment the result is recorded. In busy QC laboratories processing high volumes of incoming material, that workflow also needs to be efficient – fast enough to keep pace with production demands without compromising the integrity of the result. That is what the Wallace integrated PRI testing system is designed to deliver.

If you have questions about PRI testing, instrument selection, calibration or service, the Wallace technical team is happy to help. Contact them with your questions.

]]>